CASTING AND FOUNDING.

347

microscope, and when the alloy had been made bymixing 2.74 copper with 1 of zinc, and the loss inmelting amounted to -rasth of the whole, the con-tinuity of the line was not broken in that range oftemperature; according, however, as the proportionof the zinc was more or less, the expansion of the brassbar was greater or less than that of speculum metal.

Speculum metal and brass cannot be solderedtogether by the ordinary methods, except on a verysmall scale. Dut they may be soldered by first fittingthe brass and speculum metal nicely together byfitting or grinding. The brass is then to be tinnedand suffered to cool. Scrape the surface of the spe-culum metal lightly all over with a sharp chisel;then place the two surfaces in contact, and a slightpressure may be applied after the fusion of the tin,and continued until it is again solid. The tem-perature should then be gradually raised till the tinmelts; and then, but not till then, resin is appliedin fusion, and also a little melted tin. If resin ortin be applied in the solid state, owing to their rapidabsorption of heat in becoming fluid, they will crackthe speculum metal. The surfaces may be slightlyseparated, so as to ascertain that the speculum metalis tinned all over, which will be the case when thetemperature reaches 400°. The whole must then besuffered to cool gradually.

In easting the alloy of zinc and copper some pre-cautions are necessary to prevent so much of thezinc being volatilized, and thus producing speculummetal of varying and uncertain composition. Char-coal in fine powder must he spread over the surfaceof the metal in the crucible in a layer 2 inches thick,and occasionally renewed by throwing it in, foldedup in paper. With this precaution the loss will beabout-^th, and almost exactly the same each casting.

The proportions of zinc and copper having beendetermined, the brass-work was first cast. Thefigures will show how the materials were disposed of.Fig. 545 represents one-eighth part of the whole seen

Fig. 546 . Fig. 547 .

w

in the reverse, a single casting. Fig. 547, the wholespeculum also seen in the reverse; and Fig. 546 seenon the opposite side, previous to the soldering on of

Fig. 548 . Fig. 549 .

the plates of speculum metal; Fig. 548, the speculumcomplete, faced with 16 plates of speculum metal.The whole depth of the brass-work was 5J inches,and weighed about 450 lhs. The sides I B, Fig. 545,were made square and true, and then tinned, and thewhole bolted together with iron bolts. The tempera-ture was then raised till the tin was in fusion, and

the bolts tightened to the utmost, so as to make closejoints. In this state the speculum was turned, platedwith speculum metal and polished. A flexure was,however, observed in this speculum, and it was sup-posed that the solder was not everywhere perfect.The plates of speculum metal were therefore takenoff, and the joints secured by bedding the whole massof brass-work in casting-sand; over it there wereabout 3 inches of sand. The sand was then removedfrom the centre, so as to expose a circular surface about1^ inch diameter, and about 45 lbs. of very hotmelted brass, in the same proportions as the brassspecidum, were poured upon it in a continuous streamfrom a height of about 10 inches; the sand havingbeen so arranged that after the melted brass hadreached the depth of 2 inches, the remainder con-tinued to flow off. The melted brass soon fused thecold metal, and perfectly united with it at the placewhere it was poured. This was repeated in 34different places, marked by dots in the figures. Itwas also tried in the places marked c c, but failed.When the redundant brass had been removed with asaw, and the surface made smooth, a slight hair crackwas perceptible at the boundary of the fused metal,proceeding no doubt from expansion and contractionafter the brass had ceased to be fluid, but before ithad become ductile. This process is used by thebrass-founder in stopping holes in defective castings;he calls it burning. To secure the joint at c c holesabout 1^ inch diameter were bored completely throughat c, and the intermediate brass chiselled out. Theywere then filled with melted brass, which was easilydone by imbedding the whole in sand; clearing thesand completely out of the spaces, and pouring thebrass into each through a hole in a flat surface ofsand packed in a small flask; when the brass cooled,the contraction was sufficient to draw the joint firmlytogether. As any further yielding in the joints wasnow judged to he impossible, the speculum was againplaced on the lathe and turned to a radius of 54 feet,and new plates of speculum metal prepared for it.

Although none of these plates exceeded 9 inchessquare, much difficulty was experienced in castingthem. When cast in sand they were seldom freefrom flaws, and although cooled very slowly wereextremely brittle, sometimes flying in pieces themoment they were touched, and generally breakingin attempting to heat them for soldering. As thebroken pieces of these plates did not fit each other,the metal had evidently been in a state of tension,owing to the edges of the plates becoming solidsooner than the centre. If it w r ere possible toabstract the heat rapidly and equally from the lowersurface of a fluid disk of speculum metal, so that itshould solidify from the bottom upwards in thinlaminse, the surface being the last to solidify, a perfectcasting would be obtained; for the particles in thatcase being deposited in such a way as to fill up theinterstices, there would be no flaws; but the tem-perature being uniform in a horizontal direction, andin the vertical varying in regular gradation from thelower surface to the upper, there would be no strain.