ARSENIC.— Arsenious Acid.

oxidation of all that was contained in the soot, andsubsequent separation of the condensable oxide ofarsenic) is collected in another set of chambersexactly like those above figured; and there may bethe same looping of two lines of chambers ■whichshall alternately be cleared out.

The arsenious acid as thus obtained is a beau-tifully white minutely - crystalline substance; ithangs on the walls and roofs of the chambers, andaccumulates on the floor in glittering masses. Afterbeing collected it has to be prepared for the marketby grinding in a mill just like a flour mill, fromwhich, indeed, it comes out exactly like flour tolook at. From the mill it goes to a hopper witha leather hose attached, which hose has at its enda collar and screw, by which it is fastened to' thekeg in which the white arsenic is to be packed;by a series of light blows on the cask the materialis shaken down hard till the keg is thoroughly full,when it will hold 3 cwts. or 8£ cwts.; it is thenready for carriage.

In dealing in all these ways with such a poisonoussubstance as arsenious acid, certain precautions arenecessary. The way in which it affects the men atthe furnaces, &c., is in producing sores wherever itmay collect and be allowed to stay. The men some-times smear their faces with fuller’s earth as a pro-tection ; without that the bad effects may be kept offby thorough cleanliness, by careful washing when theday’s work is over.

With regard to the harm that may be done to theneighbourhood by the escape of arsenious acid fromthe stack, this has probably in many cases been con-founded with that which arises from the sulphurousacid gas that spreads from the same stack; the cham-bers should be of length sufficient to intercept nearlyall the arsenic.

Manufacture of White Arsenic Glass. —Whitearsenic glass is arsenious acid in an amorphous vit-reous form. At the ordinary pressure of theatmosphere, arsenious acid volatilizes from the solidform, and solidifies at once from its vapour at thetemperature of 185° C. (365° Fahr.); but it wouldseem that, under a slightly increased pressure, thevapour on condensing becomes for a moment aliquid, or we may say that, on solidifying from thegaseous state, it pastes through the liquid stage, andhence the product is vitreous. The increasedpressure causes the fusing and volatilizing tempera-tures to be distinct. Such, at all events, is ourexplanation of the result of the process now tobe described. It consists of a re-sublimation ofthe white arsenic under new conditions. There aretwo somewhat different ways of effecting this.We will first describe the one followed at Swan-sea, in Wales . Fig. 10 represents the apparatusthere employed. It consists of a cast-iron pan, 2ft. across, surmounted by a bell of the samematerial, 2 ft. G in. high. The pan is fixed perman-ently over a fire, the bell is removable. The bellbeing adjusted as in the figure, and the pan beingheated to a cherry-red heat, a charge of about jcwt. of refined white arsensic is introduced through

a hole in the top of the bell by the funnel marked a ;the hole is then stopped by the plug h. The arseniousacid soon sub-limes, and, on Fi s- to.

account of theheat of the va-pour tinder acertain amount ofpressure, it is de-posited on theinside of the ironbell in an amor-phous state — asa transparentglass, that whichis an article ofcommerce underthe name ofwhite arsenic

ass. As soonas the first chargehas been workedoff (and one canascertain thestate of it by in-troducing an ironrod through theplug-hole), another is introduced. The plug also maybe from time to time removed to relieve the pressureif it should be too great; or if the fire becomes toohot, the brick c may be removed. For the first chargeto be thus sublimed and condensed about two hoursis required; the time necessary increases to three orfour hours as the bell acquires a thicker cake. At theend of twenty-four hours the bell, with its contents,are removed, and a cold one takes its place; the arsenicglass formed inside the bell is about 1 inch thick; itis broken out and put in casks for transportation.

The method followed at Reichenstein, in Silesia, issomewhat different, though proceeding on the sameprinciple. There the product of the roasting in themuffle furnace above described is submitted to treat-ment, which will be understood from the subjoineddrawing, Fig. 11.

The part A is a front view, while B is a section ofthe apparatus employed, a, a, are the fire-grates,6, h, the ash-pits, c, c, the doors; the smoke from thevarious fire-places is carried off by the chimney, g ;e, e, are subliming-pots of cast iron, into each ofwhich a weight of about 3^ cwts. of the flour ofarsenic is introduced; they are surmounted by theiron drums, h, h, and by the caps, i, i, which in theirturn are covered by pipes, k, k, the narrow ends ofwhich enter the condensing chamber, L. The potsbeing charged, the cylinders, h, h, are placed uponthem by the aid of the handles with which they arefurnished, and the joints being well luted with acomposition of loam, hair, and blood, the caps, t, i,and the pipes, k, k, are adjusted, and, lastly, the fireis lighted. A very gentle heat is applied for abouthalf an hour, after that time the heat is somewhatincreased. If the heat be too feeble, the sublimateproduced is similar to what was put in; if it bo too